KOMPOSISYON SA KEMIKAL
Mn% | Sn% | Cu% | |
Nominal nga Komposisyon | 7 | 2.5 | Si Bal. |
PISIKAL NGA MGA PROPERTI
Densidad g/cm3 | 8.5 |
TCR 10-6/K | ± 10 |
Elastic Modulus GPa | 125 |
Thermal Conductivity W/(m·K) | 35 |
Thermal expansion coefficient 10-6/K | 21.6 |
EMF μV/K | -1 |
Resistivity Ohm mm2/m | 0.29+/-0.04 |
MEKANIKAL NGA MGA PROPERTI
Estado | Paghatag kusog | Kusog sa tensile | Elongation | Katig-a |
Mpa | MPa | % | HV | |
R350 | - | 350 | 30 | 70 |